W-O deposits with complex morphologies and significant He contents will growth on the surface of plasma facing components exposed to He discharges. To mimic the re/co-deposition process, W-O coatings were loaded with He by implanting He+ ions on W films grown by pulsed laser deposition (PLD). The use of appropriate PLD experimental parameters such as pressurised Ar or He background atmospheres induces the deposition of porous or compact W structures enhancing afterwards the gathering of different amounts of O under exposure to atmospheric air. After multiple ion implantation stages using 150 keV, 100 keV and 50 keV incident He+ ion beams with a total fluence of 5 × 1017 ion/cm2, significant amounts of He were identified in porous coatings by Rutherford backscattering (RBS). Time-of-flight elastic recoil detection (ToF-ERDA) measurements showed that most of the implanted He was already released from the porous coatings five month after implantation, while for the case of compact layers the He content remains significant at deeper layers and smoothly decrease towards the surface, as result of a different morphology and nanostructure. The proposed method involving PLD and ion implantation seems adequate to produce W-O films load by He that may be used as reference samples for fusion investigations.
Item Type: |
Article
|
Additional Information: |
This work has been carried out within the framework of the EUROfusion Consortium and has received funding from the Euratom research and training programme 2014-2018 under grant agreement No 633053. The activity was performed in the scope of the WP PFC programme. IST also received financial support from "Fundacao para a Ciencia e a Tecnologia"through project UID/FIS/50010/2013. The views and opinions expressed herein do not necessarily reflect those of the European Commission. |
Uncontrolled Keywords: |
PLD; W coatings; Ion implantation; Helium load |
Subjects: |
NATURAL SCIENCES > Physics |
Divisions: |
Division of Experimental Physics |
Depositing User: |
Ivančica Bogdanović Radović
|
Date Deposited: |
31 Mar 2020 08:30 |
URI: |
http://fulir.irb.hr/id/eprint/4229 |
DOI: |
10.1016/j.surfcoat.2018.02.089 |
Actions (login required)
|
View Item |
4229
WOS:000449896800033